e01.org

Delamination

under compression load Delamination is a mode of failure where a material fractures into layers. A variety of materials, including laminate composites and concrete, can fail by delamination. Processing can create layers in materials, such as steel formed by rolling and plastics and metals from 3D printing which can fail from layer separation. Also, surface coatings, such as paints and films, can delaminate from the coated substrate. In laminated composites, the adhesion between layers often fails first, causing the layers to separate. For example, in fiber-reinforced plastics, sheets of high strength reinforcement (e.g., carbon fiber, fiberglass) are bound together by a much weaker polymer... Source: e01 Encyclopedia. Licence: CC BY-SA 4.0.

under compression load]] Delamination is a mode of failure where a material fractures into layers. A variety of materials, including laminate composites and concrete, can fail by delamination. Processing can create layers in materials, such as steel formed by rolling and plastics and metals from 3D printing which can fail from layer separation. Also, surface coatings, such as paints and films, can delaminate from the coated substrate. In laminated composites, the adhesion between layers often fails first, causing the layers to separate. For example, in fiber-reinforced plastics, sheets of high strength reinforcement (e.g., carbon fiber, fiberglass) are bound together by a much weaker polymer matrix (e.g., epoxy). In particular, loads applied perpendicular to the high strength layers, and shear loads can cause the polymer matrix to fracture or the fiber reinforcement to debond from the polymer. Delamination also occurs in reinforced concrete when metal reinforcements near the surface corrode. The oxidized metal has a larger volume causing stresses when confined by the concrete. When the stresses exceed the strength of the concrete, cracks can form and spread to join with neighboring cracks caused by corroded rebar creating a fracture plane that runs parallel to the surface. Once the fracture plane has developed, the concrete at the surface can separate from the substrate. Processing can create layers in materials which can fail by delamination. In concrete, surfaces can flake off from improper finishing. If the surface is finished and densified by troweling while the underlying concrete is bleeding water and air, the dense top layer may separate from the water and air pushing upwards. In steels, rolling can create a microstructure when the microscopic grains are oriented in flat sheets which can fracture into layers. Also, certain 3D printing methods (e.g., fused deposition) builds parts in layers that can delaminate during printing or use. When printing thermoplastics with fused deposition, cooling a hot layer of plastic applied to a cold substrate layer can cause bending due to differential thermal contraction and layer separation. G_Q = \frac{3mP^{2}_{\max}a^{2}_{0}}{2B} where B is the thickness of the specimen and P_{\max} is the max load and m is a fitting parameter. m is determined by experimental results with a least squares fit of compliance C vs. the crack length cubed a^3 with the form of C = A + ma^3 . The candidate fracture toughness G_Q equals the mode II fracture toughness G_{IIc} if strain energy release rate falls within certain percentage of G_Q at different crack lengths specified by ASTM. \frac{P}{Q} = \frac{S_2}{S_1} = \lambda , where S_1 and S_2 are the lengths from the inner pin to the applied point load and from the outer pin to the applied point load, respectively. The normal stress in the sample \sigma_{xx} is maximized at the locations of the inner pins, and is equivalent to \sigma_{xx} = \frac{6(\lambda-1)FL}{(1+\lambda^2)bt} , where F is the total applied load on the sample, L is the sample length, b is the sample width (into the page as seen in a 2D free-body diagram), and t is the sample thickness. The shear stress \sigma_{xz} in the sample is maximized in between the inner span of the pins and is given by \sigma_{xz} = \frac{3(1- \lambda)F}{2(1+ \lambda)bt} . The ratio of normal to shear stress in the sample C is given by C = \frac{\sigma_{xx}}{\sigma_{xz}} = \frac{4L}{(1+\lambda)t} . This ratio is dependent both on the loading factor of the sample and its length-thickness ratio; both of these quantities are important in determining the mode of failure of the sample in testing.

source: e01 Encyclopedia · licence: CC BY-SA 4.0 · page · source revision

Cite this

"Delamination". 1763172766. e01 Encyclopedia. CC BY-SA 4.0. https://en.wikipedia.org/w/index.php?oldid=1322235681

JSON record · API collection · BibTeX · RIS · CSL-JSON · citation policy

Save to pass ·